◆技术指标
性能 |
指标 |
实验方法 |
拉伸强度 |
≥12MPa |
ASTM D 2671 |
断裂伸长率 |
≥300% |
ASTM D 2671 |
热老化后拉伸强度 |
≥8.4MPa |
158℃×168h |
热老化后断裂伸长率 |
≥100% |
158℃×168h |
轴向变化率 |
-8%~+8% |
ASTM D 2671 |
阻燃性 |
30秒自熄 |
SAE-AMS-DTL-23053/4 |
耐电压(额定电压600V) |
2500,1min不击穿 |
UL224 |
击穿强度 |
≥15MV/mm |
ICE 60243 |
体积电阻率 |
≥1014Ω·cm |
ICE 60093 |
◆规格表
规格 |
收缩前内径mm |
全缩后尺寸mm |
标准包装(米/根) |
|
内径 |
壁厚 |
|||
10.2/3.0 |
≥ 10.2 |
≤ 3.0 |
1.75 ± 0.25 |
1.22 |
16/5.0 |
≥ 16.0 |
≤ 5.0 |
1.90 ± 0.25 |
1.22 |
19.1/5.6 |
≥ 19.1 |
≤ 5.6 |
2.45 ± 0.25 |
1.22 |
25/8 |
≥ 25.0 |
≤ 8.0 |
2.45 ± 0.25 |
1.22 |
28/9 |
≥ 28.0 |
≤ 9.0 |
2.60 ± 0.25 |
1.22 |
35/10.2 |
≥ 35.0 |
≤ 10.2 |
2.70 ± 0.25 |
1.22 |
38.1/12 |
≥ 38.1 |
≤ 12.0 |
2.70 ± 0.25 |
1.22 |
43.2/12.7 |
≥ 43.2 |
≤ 12.7 |
2.70 ± 0.25 |
1.22 |
55/16 |
≥ 55.0 |
≤ 16.0 |
2.80 ± 0.30 |
1.22 |
63/19 |
≥ 63.0 |
≤ 19.0 |
3.00 ± 0.30 |
1.22 |
75/22 |
≥ 75.0 |
≤ 22.0 |
3.00 ± 0.30 |
1.22 |
85/25 |
≥ 85.0 |
≤ 25.0 |
3.30 ± 0.30 |
1.22 |
95/29 |
≥ 95.0 |
≤ 29.0 |
3.70 ± 0.35 |
1.22 |
115/34 |
≥ 115 |
≤ 34.0 |
3.70 ± 0.35 |
1.22 |
140/42 |
≥ 140 |
≤ 42.0 |
3.70 ± 0.35 |
1.22 |
邹经理:13825446558 (微信同号)
公司电话:400-8018-272
企业邮箱:5126108@qq.com
地址: 惠州市江北云山东路21号TCL云山工业区A栋 | 深圳市坪山区坑梓街道金沙社区青排新村二巷9号